MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

LyondellBasell Adsyl RC129L ST Thermoplastic Polyolefin
Categories: Polymer; Thermoplastic; Polyolefin

Material Notes: Adsyl RC129L ST is an advanced polyolefin, specially designed for use as a sealing layer in coextruded film applications. This grade features a low seal initiation temperature. It contains anti-blocking additives.

Availability: Africa-Middle East; Asia-Pacific; Australia and New Zealand; Europe; North America; South & Central America

Application: Barrier Film; Clarity Film; Food Packaging Film; Lamination Film; Specialty Film

Market: Flexible Packaging

Processing Method: BOPP; Cast Film; Double Bubble

Attribute: Good Optical Properties; Medium Antiblocking; Medium Temperature Heat Sealability; Metallizeable; Superior Optical Properties; Terpolymer

Information provided by LyondellBasell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.900 g/cc0.0325 lb/in³Method A; ISO 1183-1
Melt Flow 5.50 g/10 min
@Load 2.16 kg,
Temperature 230 °C
5.50 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ISO 1133-1
 
Mechanical PropertiesMetricEnglishComments
Heat Seal Strength Initiation Temperature 115 °C
@Thickness 0.0300 mm
239 °F
@Thickness 0.00118 in
 
Thermal PropertiesMetricEnglishComments
Melting Point 130 °C266 °FISO 11357-3
Vicat Softening Point 111 °C232 °FA/50; ISO 306
 
Optical PropertiesMetricEnglishComments
Haze 0.900 %
@Thickness 1.27 mm
0.900 %
@Thickness 0.0500 in
ASTM D1003
Gloss 91.0 %91.0 %45°; ASTM D2457

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PEQS9028 / 323956

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.