Applications PETROTHENE NA 324 is a series of homopolymer resins specifically designed for overwrap packaging. NA 324 provides excellent optical properties and good stiffness for improved machineability.
Regulatory Status NA 324 meets the requirements of the Food and Drug Administration regulation, 21 CFR 177.1520. This regulation allows the use of this olefin polymer in "…articles or components of articles intended for use in contact with food…" Specific limitations or conditions of use may apply.
Processing Techniques Specific recommendations for processing NA 324 can only be made when the processing conditions, equipment and end use are known.
Physical Properties These are typical values and not to be construed as specific product limits.This product is from the former Equistar product line. |