Metocene HM2089 is a single site polymerized polypropylene for film applications and Thermoforming applications. Metocene HM2089 doesn’t contain nucleated, or film additivations. Metocene HM2089 is suitable for food contact. Films produced with Metocene HM2089 will show very good stiffness and clarity. Product Features: High transparency and gloss/ High stiffness/ High purity/ Lower sealing temperature/ Energy saving/ Low volatile, clean running Typical Applications: Film applications/ Thermoforming applications/ Extrusion of films for lamination Information provided by PolyMirae |