MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Angst+Pfister APSOplast® VESPEL PI SP22 PI + 40% graphite
Categories: Polymer; Thermoplastic; Polyimide, Thermoplastic; Thermoplastic Polyimide, Graphite Filled

Material Notes: The addition of 40% graphite improves the sliding behavior and decreases the coefficient of thermal expansion. This is particularly important in the case of applications where a low coefficient of thermal expansion is more important than strength, which is slightly reduced in this case.

Information provided by Angst + Pfister

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.65 g/ccDIN EN ISO 1183-1
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 52.0 MPaASTM D 1708
Elongation at Break 3.0 %ASTM D 1708
Modulus of Elasticity 4.83 GPaASTM D 790
Coefficient of Friction 0.27p=0.05 N/mm2, v=0.6 m/s, against hardened and polished steel
 
Thermal PropertiesOriginal ValueComments
CTE, linear 27.0 µm/m-°C
@Temperature 23.0 - 60.0 °C
Thermal Conductivity 0.890 W/m-K
Maximum Service Temperature, Air 300 °Clong term
 360 °Cshort term
Flammability, UL94 V-0
 
Descriptive Properties
Coloranthracite

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PANGP072 / 250570

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.