MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Syensqo (Solvay Specialty Polymers) RHODOLINE® 1010 Surfactant
Categories: Fluid

Material Notes: Standard Applications: RHODOLINE® 1010: Because of the high defoaming efficiency of RHODOLINE® 1010, most systems require only 10 to 150 parts of defoamer per million parts of foaming system. A good starting point is to add about 100 parts of RHODOLINE® 1010 (as supplied) per million parts of foaming system. The level of foam control obtained at this concentration will determine whether to increase or decrease the concentration. RHODOLINE® 1010 may be added to the foaming system as received, or predispersed in water.

Chemical Name: WATER BASE DEFOAMER

Information provided by Solvay

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.990 - 1.01 g/ccRP-17617
Solids Content 15 - 16 %Oven, 1 hr, 1 g @ 105°C; RP-0540
pH 8.5 - 9.0RP-0420
Viscosity 200 - 500 cP#2 sp @ 30 rpm; RP-0596
 
Processing PropertiesOriginal ValueComments
Shelf Life 6.00 Month
 
Descriptive Properties
AppearanceOff White Opaque LiquidRP-0064

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSOLVAY794 / 218522

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.