MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

MOL Group BRALEN+ FA 03-01 LDPE, Film Grade
Categories: Polymer; Thermoplastic; Polyethylene (PE); Low Density (LDPE); Low Density Polyethylene (LDPE), Film Grade

Material Notes: Description: BRALEN+ FA 03-01 is a film grade of low density polyethylene with good processability, flexibility, toughness and good tear strength. This grade is additives free.

Applications: BRALEN+ FA 03-01 is designed for production of heavy duty and shrink films. It is well suited for blow molding of various containers, bottles, pipes, sheets and profiles extrusion and for injection molding. Recommended film thickness is 0.07 to 0.22 mm.

(1) Density has been measured on pressed mould specimen according to internal method. (2) Film properties tested using 50 µm thick blown film extruded at melt temperature of 200 °C and blow up ratio 2.5:1. (3) Typical properties measured on standard injection molded test specimen according to ISO 294-1.

Information provided by Molgroup Chemicals

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.920 g/cc0.0332 lb/in³1; ISO 1183-1
Melt Flow 0.30 g/10 min
@Load 2.16 kg,
Temperature 190 °C
0.30 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ISO 1133-1
Storage Temperature <= 40.0 °C<= 104 °F
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 45453; ISO 868
Tensile Strength 16.0 MPa2320 psi3; ISO 527-1,2
Film Elongation at Break, MD 500 %500 %2; ISO 527-1,3
Film Elongation at Break, TD 570 %570 %2; ISO 527-1,3
Dart Drop Test 290 g0.639 lb2; ISO 7765-1 method A
Film Tensile Strength at Break, MD 26.0 MPa3770 psi2; ISO 527-1,3
Film Tensile Strength at Break, TD 27.0 MPa3920 psi2; ISO 527-1,3
 
Thermal PropertiesMetricEnglishComments
Vicat Softening Point 93.0 °C199 °F3; ISO 306/A 50
 
Optical PropertiesMetricEnglishComments
Haze 9.5 %9.5 %2; ASTM D 1003
 
Processing PropertiesMetricEnglishComments
Processing Temperature 170 - 220 °C338 - 428 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PMOLG000 / 297166

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.