MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Steatite (Magnesium Silicon Oxide)
Categories: Ceramic; Oxide; Magnesium Oxide; Silicon Oxide

Material Notes: Magnesium silicon oxide. Used for high frequency, low loss, high voltage insulation (resistor forms, surge arrestors, standoffs, spacers, and coil forms). Less expensive than alumina insulators.

Information below is typical for commercially available steatite. A wide variation of properties is possible between specific grades.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 2.50 g/cc
Water Absorption 0.010 %
 
Mechanical PropertiesOriginal ValueComments
Hardness, Mohs 7.5
Tensile Strength, Ultimate 65.0 MPa
Modulus of Elasticity 100 GPa
Flexural Strength 125 MPa
Compressive Strength 500 MPa
Poissons Ratio 0.24
Shear Modulus 45.0 GPa
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 1.00e+11 ohm-cm
Dielectric Constant 5.9
Dielectric Strength 9.00 kV/mmWide Variation Between Grades
 
Thermal PropertiesOriginal ValueComments
CTE, linear 8.00 µm/m-°C
@Temperature 20.0 - 700 °C
 8.50 µm/m-°C
@Temperature 20.0 - 1000 °C
Specific Heat Capacity 1.00 J/g-°C
Thermal Conductivity 3.00 W/m-K
Maximum Service Temperature, Air 1000 °C
 
Descriptive Properties
ColorOff-White

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Fused Quartz
Yttria Stabilized Zirconia, YSZ
Cordierite, 2MgO-2Al2O3-5SiO2
Mullite, 3Al2O3-2SiO2
Overview of materials for Nylon 12

BSTEAT / 290

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.