Polypropylene Talc-Filled, Scratch Resistant Impact Copolymer Applications: Formulated for Interior Trim Automotive Applications The nominal properties reported herein are typical of the product but do not reflect normal testing variance and therefore should not be used for specification purposes. Data provided by Phillips Sumika Polypropylene Company (PSPC). Phillips Sumika Polypropylene Company has been shut down, as announced in 2011. This product had been discontinued prior to the shutdown announcement. |