MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Titanium 1100 Beta Quenched and annealed
Categories: Metal; Nonferrous Metal; Titanium Alloy; Alpha/Near Alpha Titanium Alloy

Material Notes:

Key Words: Titanium 1100
Vendors: Visit metalmen for your metals needs. Products include special chemistry, tight tolerances, custom tempers, odd dimensions/forms, and small quantities. Phone 1-800-767-9494.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 4.50 g/cc0.163 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 1010 MPa146000 psi
 750 MPa
@Temperature 400 °C
109000 psi
@Temperature 752 °F
Tensile Strength, Yield 910 MPa132000 psi
 625 MPa
@Temperature 400 °C
90600 psi
@Temperature 752 °F
Elongation at Break 11 %11 %
Modulus of Elasticity 107 - 117 GPa15500 - 17000 ksi
Poissons Ratio 0.310.31Typical for alpha titanium alloy.
Fatigue Strength  250 MPa
@# of Cycles 1.00e+7
36300 psi
@# of Cycles 1.00e+7
notched with Kt = 3.0.
 655 MPa
@# of Cycles 1.00e+7
95000 psi
@# of Cycles 1.00e+7
notched with Kt = 1.0.
Fracture Toughness 63.0 MPa-m½57.3 ksi-in½K(IC) after 1095ºC anneal
Shear Modulus 42.7 GPa6190 ksiCalculated from typical values.
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.000160 ohm-cm0.000160 ohm-cmEstimated from similar alpha titanium alloys.
 
Thermal PropertiesMetricEnglishComments
CTE, linear 9.00 µm/m-°C
@Temperature 20.0 - 100 °C
5.00 µin/in-°F
@Temperature 68.0 - 212 °F
Typical alpha titanium alloy
Specific Heat Capacity 0.525 J/g-°C0.125 BTU/lb-°FTypical value for titanium alloys.
Thermal Conductivity 7.00 W/m-K48.6 BTU-in/hr-ft²-°FEstimated from similar titanium alloys.
Beta Transus 1015 °C1859 °F
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 6.0 %6.0 %
Molybdenum, Mo 0.40 %0.40 %
Silicon, Si 0.40 %0.40 %
Tin, Sn 2.7 %2.7 %
Titanium, Ti 87 %87 %
Zirconium, Zr 4.0 %4.0 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Titanium 11 (Ti-6Al-2Sn-1.5Zr-1Mo-0.35Bi-0.1Si)
Titanium Ti-6Al-2Nb-1Ta-0.8Mo (Ti-621/0.8), Alpha-Annealed
ATI Allvac® 6-2-4-2 Titanium Alloy, Heat Treatment: 982°C (1800°F) + Age
Overview of materials for Alpha/Beta Titanium Alloy
Titanium IMI 834

MTA993 / 14143

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.