MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
ExxonMobil Exact™ 9071 Ethylene-based Plastomer Resin
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: Product Description: Exact 9071 plastomer is an ethylene butene copolymer produced using ExxonMobil Chemical's EXXPOL™ Technology, exhibiting both plastic and elastomeric properties.

Key Features:

  • PP/TPO modification.
  • EVA modification.
  • Designed as a low density and high molecular weight polymer modifier to impart impact strength and toughness.
  • Available as free flowing pellets.
Availability: Africa & Middle East, Europe, North America, Asia Pacific, Latin America and South America

All physical properties were measured from specimens cut from compression molded plaques per ASTM D 4703, Procedure A, Type I and conditioned at 23°C for a minimum of 40 hours per ASTM D 618 prior to testing. All stress/strain tests used specimens cut with a Type IV (Die C) die and tested with a grip separation of 25 mm (1") and a crosshead speed of 20 in./min.

Information provided by ExxonMobil Chemical.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.870 g/ccASTM D1505
Melt Flow 0.50 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ISO 1133
 0.50 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 68
@Time 15.0 sec
0.12 in; ASTM D2240
Tensile Strength at Break 4.00 MPaASTM D412 and ISO 37
Tensile Stress at Strain 2.20 MPa
@Strain 100 %
ASTM D412 and ISO 37
Elongation at Break 1500 %ASTM D412 and ISO 37
Flexural Modulus, 1% Secant 12.6 MPaASTM D790 and ISO 178
 
Thermal PropertiesOriginal ValueComments
Heat of Fusion 52.0 J/gCrystallinity; ExxonMobil Method
Melting Point 50.0 °CPeak; ExxonMobil Method
Crystallization Temperature 38.0 °CExxonMobil Method
Vicat Softening Point 56.0 °CASTM D1525 and ISO 306/A
Glass Transition Temp, Tg -49.0 °CExxonMobil Method

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Lubrizol Advanced Materials PEARLBOND® DIPP-539 Linear Thermoplastic Polyurethane
ExxonMobil Exact™ 9371 Ethylene-based Plastomer Resin
Eastman Eastar GN071 Natural PETG Copolyester
ExxonMobil Escorene® LD-752 EVA Copolymer for Specialty Applications
ExxonMobil Exact™ 9061 Ethylene-based Plastomer Resin

PEXA902 / 125945

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.