Hostacom ERC 2017L C C11658 is a mineral filled PP copolymer with medium melt flow rate and good scratch resistance. Product is UL certified. Availability: Asia-Pacific; Europe Market: Electrical / Electronics Processing Method: Injection Molding Information provided by LyondellBasell. |