MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

(Viewing data as-entered. Click here to return)
Eastman Regalrez™ 1085 Hydrocarbon Resin
Categories: Other Engineering Material

Material Notes: Product Description: Regalrez™ 1085 hydrocarbon resin is produced by polymerization and hydrogenation of pure monomer hydrocarbon feedstocks. It is highly stable, light colored, low molecular weight, nonpolar resin suggested for use in adhesives, coatings, sealants, and caulks. Regalrez™ 1085 is especially suited to applications where the lowest color and most stability against weathering and thermal degradation is required. Regalrez™ 1085 is suggested for use in elastomeric sealants and adhesives tapes where outdoor exposure will occur or where clarity and resistance to yellowing is a requirement. Due to its relatively low softening point Regalrez™1085 is especially useful in formulating systems designed to perform at low service temperatures such as freezer labels or exterior-use sealants. Regalrez™ 1085 contians no added antioxidants of UV stabilizers.

Application/Uses:

  • Assembly
  • Automotive
  • Building and Construction
  • Caulks and Sealants
  • Hot Melt Adhesives
  • Nonwovens
  • Pressure sensitive adhesives
  • Rubber and Plastic Modification
  • Solventborne Adhesives
  • Wax Modification
Key Attributes:
  • Excellent thermal and UV stability
  • Fully hydrogenated
  • Highly stable
  • Liquid
  • Water-white color

Information provided by Eastman

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Viscosity 1000 cP
@Temperature 135 °C
Melt
 10000 cP
@Temperature 115 °C
Melt
 100000 cP
@Temperature 100 °C
Melt
Molecular Weight 680 g/molMn
 1050 g/molMw. Mw/Mn ratio = 1.5
 1500 g/molMz
 
Thermal PropertiesOriginal ValueComments
Glass Transition Temp, Tg 35.0 °C
Ring & Ball Softening Point 87.0 °CASTM E28
 
Optical PropertiesOriginal ValueComments
Gardner Color Number <= 1.0ASTM D6166
 
Descriptive Properties
Cloud Point<-40°COMSCP
 43°CDACP
 87°CMMAP

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PEATM5557 / 222751

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.