MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Solvay ALKAMIDE® C-4 Surfactant
Categories: Fluid; Other Engineering Material; Additive/Filler for Polymer

Material Notes: Chemical Name ETHOXYLATED COCONUT MONOETHANOLAMINE

CAS: 61791-08-0

Available in: Asia Pacific, Europe, Latin America and North America

Applications: ALKAMIDE© C-4 is a coconut oil based alkanolamide with good detergency. ALKAMIDE© C-4 is an effective oil in water emulsifier making it well suited for household cleaners and industrial applications. ALKAMIDE© C-4 imparts viscosity and foam boosting to personal care formulations.

Information provided by Rhodia, Rhodia has been acquired by Solvay.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.980 g/cc0.0354 lb/in³
 
Optical PropertiesMetricEnglishComments
Gardner Color Number <= 6.0<= 6.0RP-0138
 
Processing PropertiesMetricEnglishComments
Shelf Life 12.0 Month12.0 Month
 
Descriptive Properties
AppearanceClear Yellow LiquidRP-0064
CompositionAlkalinity as NaOH<2.5%, RP-0203

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Haynes Hastelloy® C-4 alloy, sheet, heat treated at 1066°C, rapid quenched
Haynes Hastelloy® C-4 alloy, sheet, aged 100 hours at 899°C
Haynes Hastelloy® C-4 alloy, plate, heat treated at 1066°C, rapid quenched
Nimonic 263, Nimocast 263 Superalloy
Nimocast 90 cast Superalloy

WRHOD020 / 137250

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.