MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

(Viewing data as-entered. Click here to return)
Invista P5M2Z-012 PP Random Copolymer, Blow Molding and Profile Extrusion
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Blow Molding Grade; Polypropylene, Extrusion Grade

Material Notes: Produced without animal derived components or phthalates

Applications: Bottles and tubing

Regulatory: FDA – 21 CFR 177.1520(c) 3.1a; USP <88> Class VI

Information provided by INVISTA.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.900 g/ccASTM D1505
Melt Flow 1.90 g/10 minASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 84.0ASTM D785
Tensile Strength, Yield 28.0 MPaASTM D638
Elongation at Yield 12.0 %ASTM D638
Flexural Modulus 820 MPaSecant; ASTM D790
 880 MPaTangent; ASTM D790
Izod Impact, Notched 70.0 J/mASTM D256
Gardner Impact >= 28.0 JASTM D5420
 
Thermal PropertiesOriginal ValueComments
Melting Point 145 - 152 °CASTM D3418
Deflection Temperature at 0.46 MPa (66 psi) 76.0 °CASTM D648
 
Processing PropertiesOriginal ValueComments
Processing Temperature 200 °CTransition, Extrusion
 205 °CMetering, Extrusion
Rear Barrel Temperature 188 °CExtrusion
Head Temperature 210 °CExtrusion
Mold Temperature 16.0 °CExtrusion
 
Compliance PropertiesOriginal ValueComments
FDA YesSee notes for details.
 YesSee notes for details.
 
Descriptive Properties
Air Pressure10 psiPre-Blow, Extrusion
 90 psiBlow Air, Extrusion

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PINVIST966 / 325414

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.