MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Zinc AC41A (Zamak 5), Cast and Aged
Categories: Metal; Nonferrous Metal; Zinc Alloy

Material Notes: The composition listed is according to ASTM B86 specifications. Conflicting sources on composition. One source gives Mg content as 0.020 - 0.05% with a footnote saying the Mg content can be as low as 0.015% as long as the Pb, Cd, and Sn contents do not exceed 0.003, 0.003, and 0.001% respectively. The same source does not list Cu as a constituent of AC41A. Another source lists the Mg content as 0.030 - 0.080%. Aged indoors 10 years. Expansion during aging: 70 µm/m. Suggested Casting Temperature 395-425°C (745-795°F).

Key Words: ASTM C41A; SAE 925; UNS Z35530 (ingot), UNS Z35531 (casting); QQ-Z-363; ASTM B240; ASTM B86, Mazak 5, Zamac5
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 6.70 g/cc
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 270 MPa
Elongation at Break 13 %in 50 mm
Charpy Impact, Unnotched 56.0 J
@Thickness 6.40 mm
6.4 mm x 6.4 mm bar
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.00000650 ohm-cm
 
Thermal PropertiesOriginal ValueComments
CTE, linear 27.4 µm/m-°C
@Temperature 20.0 °C
Specific Heat Capacity 0.420 J/g-°C
Thermal Conductivity 109 W/m-K
Melting Point 380 - 386 °C
Solidus 380 °C
Liquidus 386 °C
 
Processing PropertiesOriginal ValueComments
Casting Temperature 395 - 425 °C
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al 3.5 - 4.3 %Casting
 3.9 - 4.3 %Ingot form
Cadmium, Cd <= 0.0030 %Ingot form
 <= 0.0040 %Casting
Copper, Cu 0.75 - 1.25 %Casting
 0.75 - 1.25 %Ingot form
Iron, Fe <= 0.075 %Ingot form
 <= 0.10 %Casting
Lead, Pb <= 0.0040 %Ingot form
 <= 0.0050 %Casting
Magnesium, Mg 0.030 - 0.060 %Ingot form
 0.030 - 0.080 %Casting
Tin, Sn <= 0.0020 %Ingot form
 <= 0.0030 %Casting
Zinc, Zn 94.306 - 95.32 %As balance; Ingot per ASTM B 240
 94.258 - 95.72 %As balance; Castings per ASTM B 86

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Zinc AC41A Alloy (Zamak 5), As Cast
Zinc AG40A (Zinc Alloy 3; Zn-4Al-0.4Mg; Zamak 3), Cast and Aged
Zinc AG40A (Zinc Alloy 3; Zn-4Al-0.4Mg; Zamak 3), Cast
Zinc AC43A (Zinc Alloy 2; Zn-4Al-2.5Cu-0.04Mg; Number 2 Die Casting Alloy; Zamak 2), Die Cast
Zinc Alloy 7; AG40B; Zn-4Al-0.015Mg; Zamak7

MZn41B / 14527

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.