MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Hexcel® Redux® 335M Adhesive film for bonding metallic and composite components (0.03 psf)
Categories: Polymer; Adhesive; Film; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: Redux 335 is a film adhesive curing at 250F. It is available in a range of standard areal weights from 0.015 to 0.06 psf. It is available either unsupported or with knitted and/or matt carrier for additional glueline thickness control.

Features: Cures in 60 min at 250°F for optimum properties; Good lap shear performance at temperatures ranging from -67°F to 210°F; Excellent peel properties from -67°F to 180°F; Excellent properties in sandwich structures from -67°F to 180°F; Good performance with 250°F - curing fibre reinforced composites in either co-cure or secondary bonding pocesses; Good drape at temperatures as low as 50°F; Less than 1% volatile content.
Applications: Aluminum to aluminum bonding; Fiber-reinforced composite to composite bonding; Aluminum honeycomb sandwich bonding; Aramid honeycomb sandwich bonding.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Shear Strength 1.60 ksi
@Temperature 93.3 °C
Lap Shear
 3.50 ksi
@Temperature 60.0 °C
Lap Shear
 4.90 ksi
@Temperature 21.1 °C
Lap Shear
Peel Strength 49.0 pli
@Temperature 21.1 °C
 
Processing PropertiesOriginal ValueComments
Shelf Life 12.0 Month
@Temperature -17.8 °C
 
Descriptive Properties
Areal Weight (psf)0.03
Standard Roll (ft2)540
SupportMatt

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Hexcel® Redux® 330U Epoxy film adhesives for the bonding and finishing of composites
Hexcel® Redux® 335K Adhesive film for bonding metallic and composite components (0.03 psf)

PHEXC459 / 99278

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.