Low density polyethylene M3018-P is a specialty formulation suggested for low temperature extrusion coating applications. M3018-P has been found to exhibit good coatability and adhesion to various paper substrates when processed at melt temperatures of 204°C to 248°C. Information supplied by the manufacturer. Information from manufacturer data sheet. Eastman Chemical Company sold its polyethylene business to Westlake Chemical Corporation in Dec. 2006. This grade no longer appears in the Westlake product line. |
Good coatability and adhesion to various paper substrates |