MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Reynolds TASK® 13 (C-1515) Semi-Rigid Black Urethane Casting Resin
Categories: Polymer; Thermoset; Polyurethane, TS; Thermoset Polyurethane, Elastomer, Unreinforced

Material Notes: Product Overview: TASK™ 13 and TASK™ 14 are fast setting two-component urethanes that cure quickly to black semi-rigid plastics. TASK™ 13 has a pot life of 3 minutes and demold time of 20 minutes. TASK™ 14 offers a longer pot life (10 minutes) and demold time of 45 minutes. With a Shore value of 50D, these semi-rigid plastics are used for a variety of industrial applications including fast mold making, fast model duplication, prototyping, durable miniatures, black props and special effects, or making parts that are impact resistant. Fully cured castings are tough, durable and chemical resistant.

Information provided by Reynolds Advanced Materials

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.15 g/cc1.15 g/ccASTM D-1475
Viscosity 800 cP800 cPMixed; ASTM D-2393
Linear Mold Shrinkage 0.0050 cm/cm0.0050 in/inASTM D-2566
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 9595ASTM D-2240
Hardness, Shore D 5050ASTM D-2240
Tensile Strength, Ultimate 12.4 MPa1800 psiASTM D-638
Elongation at Break 125 %125 %ASTM D-638
 
Processing PropertiesMetricEnglishComments
Cure Time 20.0 min0.333 hourHandling Time
Pot Life 3.00 min3.00 minASTM D-2471
 
Descriptive Properties
ColorBlack
Mix Ratio100A:120Bby weight
Specific Volume24.1[cu. in./lb.]

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PREYN039 / 296740

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.