PA 6, film grade of high viscosity, lubricated, not nucleated, in compliance with FDA for food contact and acc. the German BgVV Recommendation XLIV, Section VI.A" Synthetic casings in polyamide" Application Examples: single blown and cast film, sausage casings made by double bubble stretching process Former Lanxess product line is now with Envalior. |