MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Westlake Epolene® L630-29L Branched Low Density Polyethylene Homopolymer  (discontinued **)
Categories: Polymer; Thermoplastic; Polyethylene (PE)

Material Notes: Description: Epolene L-630-29P is a branched low density polyethylene homopolymer powder with low color and medium molecular weight. It is useful as a base polymer for adhesives and coatings, color concentrate dispersions, and to provide lubricity in rubber compounding. Coatings produced with Epolene L-630-29P exhibit high gloss, low moisture vapor transmission rates, grease resistance, and good heat seal ability.
    Key Attributes:
  • Enhances paraffin wax coating properties like gloss, grease resistance, and MVTR
  • Excellent thermal stability
  • Low color
  • Medium molecular weight
  • Useful in color concentrates
    Application/Uses:
  • Automotive refinish
  • Automotive
  • Building and Construction
  • Hot Melt Adhesives
  • Packaging
  • Solventborne Adhesives
  • Wax Modification

Information provided by Westlake Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.906 g/cc
Brookfield Viscosity 1800 cP
@Temperature 190 °C
 8950 cP
@Temperature 125 °C
Molecular Weight 17000 g/mol
 
Thermal PropertiesOriginal ValueComments
Flash Point >= 343 °CASTM E136
Ring & Ball Softening Point 101 °CASTM E28
 
Optical PropertiesOriginal ValueComments
Gardner Color Number <= 1.0VCC-099
 
Descriptive Properties
Penetration Hardness4 dmmASTM D5, Needle under 100-g load for 5s @ 25 °C

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PWESF8910 / 133455

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.