MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Tosoh Tosoh Susteel® 1801-005 PPS, 30% Glass Fiber Reinforced
Categories: Polymer; Thermoplastic; Polyphenylene Sulfide (PPS); Polyphenylene Sulfide (PPS) with 40% Glass Fiber Filler

Material Notes: Benefits:
  • High weld strength- High design flexibility
  • Thermal shock resistance – Thin-walled and light weight mold products
  • Low gas during molding – Void-free and good surface products
  • Low mold stain – Mold maintenance reduction

Information provided by Tosh Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 97.8 MPa
@Temperature 1000 °C
250°C Air
 97.8 MPa
@Temperature 3000 °C
250°C Air
 143.44 MPa
@Temperature 3000 °C
85°C, 85% RH
 145 MPa
@Temperature 1000 °C
90°C Hot Water
 146.7 MPa
@Temperature 1000 °C
85°C, 85% RH
 150 MPa
@Temperature 200 °C
90°C Hot Water
 163 MPa
@Temperature 0.000 °C
90°C Hot Water
 
Descriptive Properties
Gas emission0.9 ml/g350?×30min
Stain0.0002350?×30min
Thermal shock700 times-40?×30min?150?×30min
Weld strength69 MPa1000 hrs, 90°C Hot Water
 70 MPaASTM D638
 72 MPa0 hrs, 90°C Hot Water

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PTOSOH154 / 306609

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.