MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Dow Tyril® 880B SAN  (discontinued **)
Categories: Polymer; Thermoplastic; SAN Polymer; Styrene Acrylonitrile (SAN), Molded

Material Notes: TYRIL® 880B SAN copolymer combines the high levels of chemical resistance, heat resistance and overall strength of 880 resin with improved mold flow and mold release characteristics.

Data provided by Dow Chemical.

Tyril is now a Trinseo product line; this specific grade was discontinued while still a Dow product.

Key Words: Poly(Styrene Acrylonitrile)
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.08 g/ccASTM Data
Melt Density 1.00 g/cc
Linear Mold Shrinkage 0.0050 cm/cm
Melt Flow 3.5 g/10 min
@Load 3.80 kg,
Temperature 230 °C
ASTM Data
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 76.0 MPaASTM Data
Tensile Strength, Yield 76.0 MPaASTM Data
Elongation at Break 3.0 %ASTM Data
Tensile Modulus 3.45 GPaASTM Data
Charpy Impact Unnotched 2.00 J/cm²ISO Data
 2.00 J/cm²ISO Data, Low Temp
Charpy Impact, Notched 0.200 J/cm²ISO Data
 0.200 J/cm²ISO Data, Low Temp
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 67.0 µm/m-°C
@Temperature 20.0 °C
ASTM data
Specific Heat Capacity 2.23 J/g-°C
Thermal Conductivity 0.195 W/m-K
Deflection Temperature at 0.46 MPa (66 psi) 98.0 °CUnannealed; ASTM Data
Deflection Temperature at 1.8 MPa (264 psi) 88.0 °CUnannealed; ASTM Data
Vicat Softening Point 111 °C
Flammability, UL94 HB
@Thickness 1.60 mm
Oxygen Index 18.5 %
 
Optical PropertiesOriginal ValueComments
Haze 0.45 %
Transmission, Visible 86.5 %

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Dow Tyril® 880 SAN
INEOS Styrolution Luran® 348Q Transparent SAN
Synthos DL 220NA SAN Resin
Overview of materials for Styrene Acrylonitrile (SAN), Transparent
Mocom (ALBIS) LURAN KR 2635 Styrene Acrylonitrile Copolymer

PDW185 / 34416

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.