MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Mallard Creek Polymers Ecronova® KDA 618 eco Styrene Acrylic Emulsion
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE); Styrene Butadiene Rubber

Material Notes: Ecronova® KDA 618 eco is an APEO-free styrene- acrylic dispersion, which achieves excellent wet rub resistance and high hiding power due to its high pigment wetting properties. Ecronova® KDA 618 eco is suitable for interior wall paints and is also recommended for silicate and façade paints as well as plasters.

Markets: Paints and Coatings

Applications: Interior Paints, Exterior Paints, Silicate Paints

Related Products: Ecronova KDA 788, Ecronova KDA 790, Ecronova KDA 801, Ecronova KDA 1004 eco

Information provided by Mallard Creek Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Solids Content 49 - 51 %49 - 51 %
pH 7.5 - 9.07.5 - 9.0
Viscosity 1000 - 5000 cP1000 - 5000 cP
 
Thermal PropertiesMetricEnglishComments
Glass Transition Temp, Tg 22.0 °C71.6 °F
 
Descriptive Properties
Minimum Film Formation Temperature (°C)18

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PMCP9974 / 250449

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.