MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Kraiburg TPE THERMOLAST® R RC8OGGNTRL Thermoplastic Elastomer (RC/PCR Series) Adhesion to PP
Categories: Polymer; Renewable/Recycled Polymer; Thermoplastic; Elastomer, TPE; Styrenic TPE

Material Notes: The RC/PCR series is a material solution with post-consumer recycled content (hardness dependent) for a variety of applications with adhesion to PP or for single component parts. The compounds are available in natural colors and can be colored in many different ways.

Processing Method: Injection Molding

Color / RAL DESIGN:

  • Natural
Typical applications:
  • Grommets
  • Function and design elements
  • Grip applications
  • Edge guards
  • Seals for switch boxes
  • Seals for housings
  • Fasteners
  • Caps
  • Components for irrigation systems
  • Applications for waste water systems
Material advantages:
  • Adhesion to PP
  • Sustainable material
  • Colorable
  • In-process recycling possible
  • Demolding
  • Recycling-specific raw material influences are possible

Information provided by Kraiburg TPE

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.890 g/cc0.0322 lb/in³DIN EN ISO 1183-1
Storage Temperature 15.0 - 30.0 °C59.0 - 86.0 °F
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 8080DIN ISO 48-4
Tensile Strength 6.00 MPa870 psi200 mm/min; DIN 53504/ISO 37
Elongation at Break 550 %550 %200 mm/min; DIN 53504/ISO 37
Tear Strength 18.0 kN/m103 pliISO 34-1 Method B (b)
Compression Set 45 %
@Temperature 23.0 °C,
Time 259000 sec
45 %
@Temperature 73.4 °F,
Time 72.0 hour
DIN ISO 815-1 Method A
 
Descriptive Properties
ColorNatural
Recycled raw materials content (%)33

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PKRAIA8471 / 309135

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.