MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Röhm DEGADUR® 165 Methacrylic resin
Categories: Polymer; Thermoplastic; Adhesives, Sealants, and Coatings

Material Notes: General Description: Under the DEGADUR® trademark, Röhm produces rapidly curing methacrylic resins that are used to formulate floor coatings, with the addition of fillers and pigments. Their rapid curing (even at temperatures as low as minus 30°C) ensures very short interruptions in routine operations. The coatings can be used to provide smooth or textured surfaces. Seamless DEGADUR® industrial floor coatings are robust and resistant to many conventional chemicals such as acids and alkalis. The degree of mechanical strength and slip resistance can be precisely adjusted according to the specific requirements or relevant industrial regulations. Individual wishes can be met in terms of color or design. DEGADUR® coating systems can generally be applied on concrete and metal substrates, asphalt, indoor and outdoor areas as well as in wet and dry rooms.

Decorative systems for dry areas: Coatings based on DEGADUR® 151, sealed with DEGADUR® 165, are especially suitable for easy-to-clean, decorative indoor surfaces on high-quality substrates. The DEGADUR® 165 seal coat shows particularly good resistance to chemicals and tire abrasion.

Summary of benefits

  • Rapid curing - floor can be used and exposed to normal loads after two hours, which means minimal downtimes
  • Coating possible at ambient temperatures of -30°C to +35 °C
  • Good wear resistance
  • Seamless and water-tight
  • Good chemical resistance to acids, alkalis and many cleaning agents
  • New DEGADUR® coatings can be applied to old DEGADUR® substrates
DEGADUR® 151/165 – for custom-tailored system solutions
  • Extremely hard-wearing with high compressive strength
  • High resistance to gasoline and oil
  • Good resistance to tire marks
  • For application on substrates with high mechanical strength
Fields of application:
  • Storage rooms
  • Salesrooms and exhibition rooms
  • Bakeries, cafés, beverage stores
  • Laboratories, pharmaceutical industry
  • Printing shops, distributing centers, workshops
  • Discothèques, gyms
  • Changing rooms
  • Zoo enclosures (indoors)
  • Museums
  • Banks

Information provided by Roehm America LLC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 8.80 MPa1280 psiDIN EN ISO 527
Elongation at Break 0.80 %0.80 %DIN EN ISO 527
Modulus of Elasticity 2.10 GPa305 ksiDIN EN ISO 527
Compressive Strength 44.0 MPa6380 psiDIN EN ISO 604
Adhesive Bond Strength 4.30 MPa624 psiTensile bond strength on concrete; DIN ISO 4624 ZTV-SIB
 
Descriptive Properties
Impact strength4 NmEN ISO 6272
Wear resistance according to BCA10µmprEN 13892-4

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PROHM9324 / 319941

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.