MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Akrochem Accelerator ZBED
Categories: Other Engineering Material

Material Notes: Product Description: Accelerator ZBED is an active form of Zinc Dithiocarbamate, which can be modified by MBT or MBTS, etc. It is non-staining and non-discoloring and is safer processing than Zinc Dibutyl Dithiocarbamate. In latex it is less likely to cause pre-cure at room temperature than other dithiocarbamates. However, ZBED is a typical Ultra-Accelerator at normal curing temperatures. It is also useful as a secondary accelerator for the continuous vulcanization of butyl rubber extrusions. ZBED has found usefulness in minimizing harmful nitrosoamines. The N-Nitroso dibenzylamine produced during cure is relatively non-extractable, non-volatile, and has been found to be noncarcinogenic. Zinc dibenzyl dithiocarbamate has compliance with FDA Regulation CFR 21 Part 177.2600.

Information provided by Akrochem Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.42 g/cc
 
Thermal PropertiesOriginal ValueComments
Melting Point >= 179 °C
 
Processing PropertiesOriginal ValueComments
Moisture Content <= 0.50 %
 
Component Elements PropertiesOriginal ValueComments
Zinc, Zn <= 12 %
 
Descriptive Properties
AppearanceWhite Powder
Purity>98%

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PAKZCH434 / 315352

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.