MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
HB Fuller Swift®therm 2103NA Hot Melt
Categories: Polymer; Thermoplastic; Adhesives, Sealants, and Coatings

Material Notes: Swift®therm 2103NA is a longer open time hot melt adhesive developed for industrial assembly and automotive interior applications. It will adhere to a variety of substrates and great for bonding blocked textile into PP and ABS. 2103NA is also recommended for bonding of plastics, ABS, EPDM, wires, carpets, wood, aluminum, PP, fiberboard, Lignotock, and Fibrit.

Features and Benefits:

  • Long open time
  • High green strength
  • High heat resistance
  • High strength and flexibility
  • Suitable substrates include: Bonding of EPDM, wires and carpets to wood, aluminum, PP, fiberboard, Lignotock, Fibrit, etc.

Information provided by H.B. Fuller Company

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.930 g/cc
Brookfield Viscosity 4500 cP
@Temperature 350 °C
 5300 cP
@Temperature 300 °C
Storage Temperature 15.0 - 35.0 °C
 
Processing PropertiesOriginal ValueComments
Processing Temperature 150 - 200 °C
Cure Time 210 secOpen time (4mm bead @ 200°C application temp)
Shelf Life 12.0 Month
 
Descriptive Properties
ColorTransparent
ConsistencyViscous LiquidSolid at Room Temperature

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PHBFULL165 / 316956

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.