MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Hexcel® HexPly® 922-1/35%/G926 180°C Curing Epoxy Matrix
Categories: Polymer; Thermoset; Epoxy; Epoxy Cure Resin

Material Notes: 5H satin/370g/m2 carbon fabric: FVC=60%

Information provided by HexCel

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 718 MPa104000 psiMaterial as cured; RT
 786 MPa114000 psiAfter ageing at 70°C / 95% RH; RT
 677 MPa
@Temperature 175 °C
98200 psi
@Temperature 347 °F
After ageing at 70°C / 95% RH
 774 MPa
@Temperature 175 °C
112000 psi
@Temperature 347 °F
Material as cured
Tensile Modulus 67.0 GPa9720 ksiMaterial as cured; RT
 77.0 GPa11200 ksiAfter ageing at 70°C / 95% RH; RT
 64.0 GPa
@Temperature 175 °C
9280 ksi
@Temperature 347 °F
After ageing at 70°C / 95% RH
 70.0 GPa
@Temperature 175 °C
10200 ksi
@Temperature 347 °F
Material as cured
Flexural Yield Strength 1038 MPa150500 psiAfter ageing at 70°C / 95% RH; RT
 1079 MPa156500 psiMaterial as cured; RT
 244 MPa
@Temperature 175 °C
35400 psi
@Temperature 347 °F
After ageing at 70°C / 95% RH
 761 MPa
@Temperature 175 °C
110000 psi
@Temperature 347 °F
Material as cured
Flexural Modulus 57.0 GPa8270 ksiAfter ageing at 70°C / 95% RH; RT
 60.0 GPa8700 ksiMaterial as cured; RT
 42.0 GPa
@Temperature 175 °C
6090 ksi
@Temperature 347 °F
After ageing at 70°C / 95% RH
 56.0 GPa
@Temperature 175 °C
8120 ksi
@Temperature 347 °F
Material as cured
Compressive Yield Strength 605 MPa87700 psiAfter ageing at 70°C / 95% RH; RT
 667 MPa96700 psiMaterial as cured; RT
 218 MPa
@Temperature 175 °C
31600 psi
@Temperature 347 °F
After ageing at 70°C / 95% RH
 493 MPa
@Temperature 175 °C
71500 psi
@Temperature 347 °F
Material as cured
Compressive Modulus 65.0 GPa9430 ksiAfter ageing at 70°C / 95% RH; RT
 66.0 GPa9570 ksiMaterial as cured; RT
 52.0 GPa
@Temperature 175 °C
7540 ksi
@Temperature 347 °F
After ageing at 70°C / 95% RH
 57.0 GPa
@Temperature 175 °C
8270 ksi
@Temperature 347 °F
Material as cured
Shear Modulus 5.00 GPa725 ksiIn-Plane; After ageing at 70°C / 95% RH; RT
 5.60 GPa812 ksiIn-Plane; Material as cured; RT
Shear Strength 73.0 MPa10600 psiIL; Material as cured; RT
 79.0 MPa11500 psiIL; After ageing at 70°C / 95% RH; RT
 90.0 MPa13100 psiIn-Plane; After ageing at 70°C / 95% RH; RT
 98.0 MPa14200 psiIn-Plane; Material as cured; RT
 20.0 MPa
@Temperature 175 °C
2900 psi
@Temperature 347 °F
IL; After ageing at 70°C / 95% RH
 53.0 MPa
@Temperature 175 °C
7690 psi
@Temperature 347 °F
IL; Material as cured

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Hexcel® HexPly® 922-1 180°C Curing Epoxy Matrix
Hexcel® HexPly® 924 180°C Curing Epoxy Matrix
Hexcel® HexPly® F263 Epoxy Resin
Hexcel® HexPly® F185 Epoxy Resin
Hexcel® HexPly® F155 Epoxy Resin

PHEXC067 / 98537

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.