MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
3M Dyneon™ Fluorel™ FE-5623Q Fluoroelastomer VF2 + HFP Dipolymer  (discontinued **)
Categories: Polymer; Thermoset; Fluoropolymer, TS; Thermoset Fluoroelastomer; Rubber or Thermoset Elastomer (TSE)

Material Notes: Data provided by the manufacturer, Dyneon LLC.

Incorporated cure polymer, 65.9%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, and 4% Ca(OH)2. The FE series O-ring grades are the cleanest running Dyneon O-ring grade polymers available; provide excellent mold release & improved scorch safety. This allows molding at higher temperatures (>200°C) for faster cure cycles - resulting in parts with improved dimensional stability. FE-5621Q and FE-5641Q have lower mold shrinkage. Used in O-Ring Applications.

Key Words: Vinylidene Fluoride, PVF2; Hexafluoropropylene
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.80 g/cc
Oxygen Transmission 98.0 cc-mm/m²-24hr-atm
Mooney Viscosity 23
@Temperature 121 °C
ML1+10
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 79
Tensile Strength, Ultimate 17.0 MPa
Tensile Strength, Yield 0.00730 GPaM100
Elongation at Break 180 %
Coefficient of Friction, Dynamic 0.80
Compression Set 13 %
@Temperature 200 °C
70 hr; ASTM D395B
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 1.00e+13 - 1.00e+14 ohm-cm
Dielectric Constant 11.4
@Frequency 6.00e+7 Hz
Dielectric Strength 25.0 kV/mm
 
Thermal PropertiesOriginal ValueComments
CTE, linear 200 µm/m-°C
@Temperature 20.0 °C
Specific Heat Capacity 1.65 J/g-°C
Thermal Conductivity 0.240 W/m-K
Glass Transition Temp, Tg -18.0 °CTR10

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
LNP Lubricomp® RFL-4036 HS BK8-115 Polyamide 66, Carbon Fiber Reinforced, PTFE Lubricant
Mitsubishi Chemical Advanced Materials Duratron™ T5030 PAI Polyamide-imide, glass reinforced, extruded
Overview of materials for Polyimide, Thermoset Film
3M Dyneon™ FC 2110Q Fluoroelastomer
3M Dyneon™ Fluorel™ FE-5610Q Fluoroelastomer VF2 + HFP Dipolymer

PDYN09 / 34704

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.