MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
CHT Group QM 280 80 Shore A, Addition Cure Moldmaking Material
Categories: Polymer; Thermoset; Silicone

Material Notes: Product Description: QM 280 is a two-component, room temperature, addition cure, silicone material. The cured rubber has excellent mechanical properties, good shelf-life stability, excellent physical properties and resin resistance. This material is a good choice for the molding of furniture, picture frames and architectural materials. QM 280 is exceptionally good where high durometer and dimensional stability are required.

Key Features:

  • High durometer
  • Casting resin resistance
  • Fast demold time
  • Excellent dimensional stability
Main Applications:
  • Molds for architectural replication
  • Molds for polyester, epoxy resin casting, and rigid or foam polyurethane
  • Molds for technical articles and prototypes
  • Molds for furniture and picture frame replication
  • High durometer silicone for roller applications

Formerly Amber Chemical Co (ACC Silicones), aquired by CHT in 2017

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.02 g/ccQM 280B, Uncatalyzed
 1.50 g/ccQM 280A, Uncatalyzed
Viscosity 1000 cPQM 280B, Uncatalyzed
 90000 cPCatalyzed
 140000 cPQM 280A, Uncatalyzed
Linear Mold Shrinkage <= 0.0010 cm/cmCured 3 days at 25°C
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 80Cured 3 days at 25°C
Tensile Strength 1100 psiCured 3 days at 25°C
Elongation at Break 75 %Cured 3 days at 25°C
Tear Strength 75.0 pliCured 3 days at 25°C
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 204 °CCured 3 days at 25°C
Minimum Service Temperature, Air -55.0 °CCured 3 days at 25°C
 
Processing PropertiesOriginal ValueComments
Cure Time 8.00 - 12.0 hourDemold time, Catalyzed
 72.0 hour
@Temperature 25.0 °C
Pot Life 60.0 minCatalyzed
 
Descriptive Properties
ColorBeigeQM 280A, Uncatalyzed
 BeigeCatalyzed
 ClearQM 280B, Uncatalyzed

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
ExxonMobil Santoprene® 8201-90 Thermoplastic Elastomer
Overview of materials for Silicone Rubber
Barlog Plastics KEBAFLEX E 90.1 TPE-V, Shore A90
CHT Group QLE 1037 60 Shore A, Addition Cure Elastomer for Coating Applications
CHT Group QLE 1035PLE 38 Shore A, Addition Cure Elastomer for Coating Applications

PACC2060 / 199448

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.