MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Dow Appeel™ 35D220 Polyolefin
Categories: Polymer; Thermoplastic; Polyolefin

Material Notes: Product Description: Appeel™ 35D220 is a modified polyolefin resin designed to function as a peelable sealing layer. It is most often suggested to provide interfacial peel seals film to film and occasionally for peel seal for PP and PE. It is available in pellet form for use in conventional extrusion or coextrusion equipment designed to process polyethylene resin.
Characteristics/Benefits:
  • Contains amide slip agent
  • Contains antiblock agent
Applications:
  • Interfacial Peel Seal for pouches, Peelable Lidding film to other polyolefin substrates.

    Availability: Africa & Middle East; Asia Pacific; Latin America; Europe; North America

    Additive: Antiblock; Slip

    Agency Ratings: FDA 21 CFR 177.1520 ©

    Form: Pellets

    Processing Method: Coextrusion; Extrusion

    Information provided by The Dow Chemical Company

  • Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
     
    Physical PropertiesMetricEnglishComments
    Density 0.915 g/cc0.0331 lb/in³ASTM D792
    Melt Flow 1.7 g/10 min
    @Load 2.16 kg,
    Temperature 190 °C
    1.7 g/10 min
    @Load 4.76 lb,
    Temperature 374 °F
    ASTM D1238
     
    Thermal PropertiesMetricEnglishComments
    Melting Point 105 °C221 °F

    Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

    PDOWF395 / 311088

    Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

    The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.