MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Eneos RB810 TPE
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: JSR has developed this grade as the only supplier in the world. Applications are broad. For example, the vibration absorbing materials for automobile, films, tubes, rubber shoe soles, some injection molded products and plastic modifiers.

Applications: Industrial Goods, Melt Bags, Various Sponge Products? Resin Vibration Insulators, Rubber Modifiers

ENEOS has acquired the elastomer product lines from JSR Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.900 g/cc0.900 g/cc
Linear Mold Shrinkage 0.0070 - 0.0090 cm/cm0.0070 - 0.0090 in/in
Melt Flow 3.0 g/10 min
@Load 2.16 kg,
Temperature 150 °C
3.0 g/10 min
@Load 4.77 lb,
Temperature 302 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 8282ASTM D2240
Hardness, Shore D 3232ASTM D2240
Tensile Strength 6.40 MPa928 psiASTM D412
Elongation at Break 750 %750 %ASTM D412
300% Modulus 3.90 MPa566 psiASTM D412
Izod Impact, Notched NBNBASTM D256
 
Thermal PropertiesMetricEnglishComments
Melting Point 71.0 °C160 °F
Vicat Softening Point 39.0 °C102 °FASTM D1525
Brittleness Temperature -40.0 °C-40.0 °FASTM D746
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.511.51ASTM D542
Haze 2.6 %2.6 %ASTM D1003
Transmission, Visible 91 %91 %ASTM D1003
 
Descriptive Properties
Content (%)90Microstructure, Percentage of 1,2 bonds
Product formPellet

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PJSRC8156 / 295472

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.