MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Covestro Desmopan® 372 Thermoplastic Polyurethane  (discontinued **)
Categories: Polymer; Thermoplastic; Polyurethane, TP; Thermoplastic Polyurethane (TPUR), Polyester Grade

Material Notes: Desmopan 372 is a TPU on the basis of a special ester.

Applications: Transport rolls, technical automotive parts.

Information provided by Bayer.

As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro.

Key Words: TPUR
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.24 g/cc
Moisture Absorption at Equilibrium 0.20 %50% RH
Water Absorption at Saturation 1.22 %
 1.22 %
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 73DIN 53505
Elongation at Break >= 50 %Nominal
Tensile Creep Modulus, 1 hour 455 MPa
Tensile Creep Modulus, 1000 hours 158 MPa
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 5.00e+14 ohm-cm
Surface Resistance 9.00e+14 ohm
Dielectric Constant 3.9
@Frequency 1e+6 Hz
 4.6
@Frequency 100 Hz
Dielectric Strength 23.7 kV/mm
Dissipation Factor 0.029
@Frequency 1e+6 Hz
 0.031
@Frequency 100 Hz
Comparative Tracking Index 600 V
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 130 µm/m-°C
@Temperature 20.0 °C
Deflection Temperature at 0.46 MPa (66 psi) 59.0 °C
Deflection Temperature at 1.8 MPa (264 psi) 48.0 °C
Vicat Softening Point 79.0 °C

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Arkema Kynar® 710 Polyvinylidene Fluoride Homopolymer- Injection Molding
Celanese Hytrel® 4056 TPC-ET
Lubrizol ESTANE® 58212 Ether Based Thermoplastic Polyurethane
Arkema KYNAR® 9000 HD Polyvinylidene Fluoride - Injection Molding
Syensqo (Solvay Specialty Polymers) Solef® 1008 PVDF Homopolymer

PBA104 / 26698

Polyurethane

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.