MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Nouryon Perkadox L-W75 Acrylics Dibenzoyl peroxide, 75% with water
Categories: Other Engineering Material

Material Notes: Initiator (75% active ingredient in water) for (co)polymerization of methacrylates and acrylates.

CAS number: 94-36-0

EINECS/ELINCS No.: 202-327-6

Applications: Perkadox L-W75 is an initiator (75% peroxide concentration as wet powder) for (co)polymerization of styrene, acrylonitrile, vinylacetate, methacrylates and acrylates. Also used as initiator for curing unsaturated polyester, vinyl ester and acrylic thermoset resins at ambient or slightly elevated temperatures.

Information provided by Nouryon

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density >= 0.630 g/cc>= 0.0228 lb/in³
Half-life  0.100
@Temperature 113 °C
0.100
@Temperature 235 °F
[hr]
 1.00
@Temperature 91.0 °C
1.00
@Temperature 196 °F
[hr]
 10.0
@Temperature 71.0 °C
10.0
@Temperature 160 °F
[hr]
Molecular Weight 242.2 g/mol242.2 g/mol
Storage Temperature <= 40.0 °C<= 104 °F
 
Thermal PropertiesMetricEnglishComments
Decomposition Temperature 80.0 °C176 °FSelf-Accelerating Decomposition Temperature
 
Processing PropertiesMetricEnglishComments
Shelf Life 3.00 Month3.00 Month
 
Descriptive Properties
AppearanceWhite granular powder
Assay74.0-76.0 %
Content= 2500 mg/kgInorganic + organic hydrolysable chloride
 4.88-5.02 %Active oxygen

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PNOURY817 / 286340

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.