Tosoh NIPPOLAN 3110 Adhesive
Categories:
Polymer
;
Adhesive
Material Notes:
Main Applications: Plastic films (PVC, PET, PP etc)
Solvent: Toluene/Acetone/Methyl ethyl ketone
Information provided by Tosh Corporation
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Solids Content
22 - 26 %
22 - 26 %
Viscosity
4800
-
6200
cP
4800
-
6200
cP
Mechanical Properties
Metric
English
Comments
Tensile Strength
58.0
MPa
8410
psi
Elongation at Break
700 %
700 %
100% Modulus
44.0
MPa
6380
psi
Thermal Properties
Metric
English
Comments
Softening Point
45.0
°C
113
°F
Glass Transition Temp, Tg
-15.0
°C
5.00
°F
Processing Properties
Metric
English
Comments
Shelf Life
3.00
Month
@Temperature 15.0 - 25.0 °C
3.00
Month
@Temperature 59.0 - 77.0 °F
Descriptive Properties
Appearance
Pale yellow liquid
Color
<500
APHA
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
PTOSOH173 / 306628
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.