MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Phillips 66 Syncon® 220 Synthetic EP Gear Oil, AGMA No. 5EP
Categories: Fluid; Lubricant; Polyalphaolefin (PAO)

Material Notes: Syncon EP Plus Gear Oil is a premium quality, synthetic, extreme-pressure industrial gear lubricant developed for the lubrication of enclosed gear drives and heavily loaded plain or rolling-element bearings operating at extreme temperatures or in severe service. It is suitable for use over a wider temperature range than conventional mineral oil-based gear oils. It meets the performance requirements of major gear drive manufacturers. Syncon EP Plus Gear Oil is formulated with synthetic polyalphaolefin (PAO) base oils, a viscosity modifier and a non-chlorinated extreme-pressure additive package. It has outstanding oxidation resistance and thermal stability at high temperatures to help minimize deposit formation and provide long service life. It has high load-carrying capacity for protection against scuffing and wear, protects against rust and corrosion, and is resistant to excessive foaming that can interfere with proper lubrication. It has a high viscosity index and low pour point for use in equipment operating at extreme temperatures or over a very wide temperature range.

Applications:

  • Heavily loaded enclosed gear drives, such as those found in mine hoists and mining machinery
  • Enclosed industrial gear drives operating at very low or very high temperatures, or operating continuously at higher than normal operating temperatures
  • Heavily loaded plain and rolling-element bearings operating at extreme temperatures
  • Applications where the equipment manufacturer recommends a high VI, synthetic, extreme-pressure gear oil
Syncon EP Plus Gear Oil meets the requirements of the following industry and OEM specifications:
  • ANSI/AGMA Standard 9005-E02
  • DIN 51517 Part 3, Lubricating Oils, Type CLP HC
  • German Steel Industry SEB 181226, Type CLP HC
  • ISO 12925-1:1996, Type L-CKC
  • Joy Machinery TO-SHEP (ISO VG 320), TO-SMEP (ISO VG 220)
  • U.S. Steel 224
Features/Benefits:
  • Outstanding oxidation resistance and thermal stability at high temperatures
  • Outstanding low-temperature properties
  • High viscosity index and low pour point for use over a wide temperature range
  • Excellent extreme-pressure properties
  • Protects against scuffing and wear
  • Protects against rust and corrosion
  • Non-chlorinated additive system
  • Suitable for year-round use
  • Extended service intervals compared with conventional mineral oil-based gear oils

Phillips 66 Lubricants was spun-off from ConocoPhillips in 2012.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.848 g/cc
Density 7.06 lb/gal
Viscosity Measurement 172Viscosity Index
Saybolt Viscosity at 100°F 1119 SUS
Saybolt Viscosity at 210°F 142 SUS
Kinematic Viscosity at 40°C (104°F) 218 cSt
Kinematic Viscosity at 100°C (212°F) 29 cSt
ASTM Color 1.0ASTM D1500
 
Chemical PropertiesOriginal ValueComments
Total Acid Number 0.20[mg KOH/g]; ASTM D974
 
Mechanical PropertiesOriginal ValueComments
Four Ball Extreme Pressure, Weld Load 315 kgASTM D2783
Four Ball Wear 0.360 mmScar Diameter; ASTM D4172
Timken Test 70.0 lbOK Load; ASTM D2782
 
Thermal PropertiesOriginal ValueComments
Pour Point -49.0 °F
Flash Point 464 °F
 
Descriptive Properties
ASTM Rust A&BPass
Copper Corrosion1b
FZG Scuffing Test>12 Failure Load StageASTM D5182
Oxidation Stability1.7%Viscosity Increase @ 121°C, ASTM D2893
Precipitation Number<0.05 mlASTM D91

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

WCON169 / 75206

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.