MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Mallard Creek Polymers Rovene® 4470 Carboxylated Styrene-Butadiene Emulsion
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE); Styrene Butadiene Rubber

Material Notes: ROVENE® 4470 is a carboxylated styrene-butadiene emulsion that has a very firm hand with outstanding strength properties. This binder is able to accept high filler loads of calcium carbonate, clays, and alumina trihydrate and still retain excellent tensile strength. ROVENE® 4470 is crosslinkable with external crosslinking agents. Sodium polyacrylate thickeners are commonly used to obtain the required application viscosity. In contrast to conventional SBR polymers, ROVENE® 4470 is more efficient in thickener use. It also has good aging properties, water resistance, and adhesion to a wide variety of fibers.
APPLICATIONS: ROVENE® 4470 is recommended for applications in carpet and needle-punch backcoating.

Information provided by Mallard Creek Polymers

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Solids Content 52.5 - 54.5 %
Particle Size 0.21 µm
pH 8.5 - 9.0
Brookfield Viscosity 200 - 900 cP#2/20 rpm
 
Chemical PropertiesOriginal ValueComments
Styrene Content 67 %
 
Thermal PropertiesOriginal ValueComments
Glass Transition Temp, Tg 16.0 °C
 
Descriptive Properties
EmulsifiersAnionic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Versalis Europrene® 1778 Emulsion Styrene-Butadiene Rubber
Versalis Europrene Latice® 440 Carboxylated Styrene - Butadiene Copolymer
Nitriflex SB-1006 Styrene Butadiene Copolymer
Nitriflex SB-1006 A Styrene Butadiene Copolymer
Mallard Creek Polymers BarrierPro® 4551 Carboxylated Styrene-Butadiene Emulsion

PMCP049 / 104706

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.