MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Solder Replacement
RoHS Compliant Adhesives for Solder Replacement
Master Bond offers RoHS compliant, electrically conductive systems to replace lead soldering. These epoxy and silicone adhesives offer low volume resistivity, low outgassing and high temperature resistance.

(Viewing data as-entered. Click here to return)
Lucas-Milhaupt Silvaloy® 541 Silver Based Cadmium Free Filler Metal
Categories: Metal; Nonferrous Metal; Precious Metal; Silver Alloy; Solder/Braze Alloy

Material Notes: Braze 541 is an intermediate temperature silver brazing alloy with a rather long, 235EF (130EC) melting range. It has a tendency to liquate (i.e. separate into low and high melting constituents) if heated slowly through its melting range. Therefore, it is preferable to use this alloy where the assembly can be heated rapidly to brazing temperature. The long melting range of this alloy is useful when wide gap joints are hand fed since semi-fluid alloys can be worked across the gaps.

Applications:Braze 541 is employed in numerous furnace brazing situations because of its low zinc content. The U.S. Air Force specifies it for many jet engine sub-assemblies. It is used for making joints that are subjected to elevated temperatures, ranging up to 700EF (370EC), particularly on stainless steel.

Specifications: This alloy conforms to the following specifications-AWS A5.8 BAg-13, ASME Boiler & Pressure Vessel Code Sec. II C SFA-5.8 BAg-13, SAE AMS 4772

Information provided by Lucas-Milhaupt, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 9.63 g/cc
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 30000 - 35000 psiCopper butt joint
 35000 - 40000 psiNickel-Silver butt joint
 35000 - 50000 psiBrass butt joint
Elongation at Break 2.0 - 3.0 %% in 2", Nickel-Silver butt joint
 10 - 19 %% in 2", Copper butt joint
 13 - 25 %% in 2", Brass butt joint
Shear Strength 7000 psi
@Temperature 538 °C
18-8 Stainless Steel butt joint
 15000 psi
@Temperature 399 °C
18-8 Stainless Steel butt joint
 21500 psi
@Temperature 260 °C
18-8 Stainless Steel butt joint
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.00000346 ohm-cm
 
Thermal PropertiesOriginal ValueComments
Melting Point 1340 - 1575 °F
Solidus 1340 °FMelting Point
Liquidus 1575 °FFlow Point
 
Component Elements PropertiesOriginal ValueComments
Copper, Cu 39 - 41 %
Nickel, Ni 0.50 - 1.5 %
Other, total <= 0.15 %
Silver, Ag 54 - 55 %
Zinc, Zn 4.0 - 6.0 %
 
Descriptive Properties
ColorWhite

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Lucas-Milhaupt Silvaloy® 403 Carbide Brazing Alloy
Wingate Alloys Winco 34 General Purpose Corrosion and Abrasion Resistant Stainless Steel
Lucas-Milhaupt Silvaloy® 450 Silver Based Cadmium Free Filler Metal
Lucas-Milhaupt BRAZE 402 Silver Based Cadmium Free Filler Metal
ATI Allegheny Ludlum AL 800AT™ Nickel-Base Alloy, UNS N08811

NLUCMI23 / 18090

solder replacement adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.