High performance epoxy for specialty bonding and potting applications to 350ºF (175°C). Can be applied to a myriad of substrates, offering exceptional chemical, electrical, and mechanical properties. General purpose, low viscosity, electrical potting compound. Low shrinkage and excellent dimensional stability. |
Aremco’s High Performance Epoxies provide a wide range of solutions for bonding ceramics, composites, glass, metals, plastics, and other materials. Visit us today at Aremco.com or call 1 (845) 268-0039 to speak with an engineer.Click here to view all available suppliers for this material. Please click here if you are a supplier and would like information on how to add your listing to this material. |