MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Denka GR-0500 ABS Polymer
Categories: Polymer; Thermoplastic; ABS Polymer; Acrylonitrile Butadiene Styrene (ABS), Molded

Material Notes: High rigidity Grade. Used in a wide range of applications, including toys, home articles, home electric appliances, OA equipment, exterior and interior automotive parts, etc.

Information provided by Denka Company Limited.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.05 g/cc0.0379 lb/in³ASTM D-792
 1.06 g/cc0.0383 lb/in³ISO 1183
Linear Mold Shrinkage 0.0040 - 0.0060 cm/cm
@Thickness 2.00 mm
0.0040 - 0.0060 in/in
@Thickness 0.0787 in
DENKA Method
Melt Flow 21 g/10 min
@Load 9.99 kg,
Temperature 220 °C
21 g/10 min
@Load 22.0 lb,
Temperature 428 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 118118ISO 2039-2
 121121ASTM D-785
Tensile Strength at Break 44.0 MPa6380 psi50 mm/min; ISO 527-1,-2
 55.0 MPa7980 psi5 mm/min; ASTM D-638
Tensile Strength, Yield 61.0 MPa8850 psi50 mm/min; ISO 527-1,-2
Tensile Modulus 3.05 GPa442 ksi1 mm/min; ISO 527-1, -2
Flexural Strength 91.0 MPa13200 psi15 mm/min; ASTM D-790
 98.0 MPa14200 psi2 mm/min; ISO 178
Flexural Modulus 2.90 GPa421 ksi15 mm/min; ASTM D-790
 3.00 GPa435 ksi2 mm/min; ISO 178
Izod Impact, Notched 0.590 J/cm1.11 ft-lb/inASTM D-256
Charpy Impact, Notched 0.400 J/cm²1.90 ft-lb/in²ISO 179
 
Electrical PropertiesMetricEnglishComments
Surface Resistance >= 1.00e+16 ohm>= 1.00e+16 ohm50% RH; JIS K 6911
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 83.0 °C181 °FFlatwise; ISO 75-1, -2
 91.0 °C196 °FEdgewise; ASTM D-648
Vicat Softening Point  105 °C
@Load 5.10 kg
221 °F
@Load 11.2 lb
ASTM D-1525
 107 °C
@Load 5.10 kg
225 °F
@Load 11.2 lb
ISO 306
Flammability, UL94 HBHB
 
Processing PropertiesMetricEnglishComments
Processing Temperature 180 - 200 °C356 - 392 °FCylinder 1
 190 - 220 °C374 - 428 °FCylinder 2
 200 - 240 °C392 - 464 °FCylinder 3
Nozzle Temperature 200 - 235 °C392 - 455 °F
Mold Temperature 40.0 - 60.0 °C104 - 140 °F
Drying Temperature 80.0 - 85.0 °C
@Time 7200 - 10800 sec
176 - 185 °F
@Time 2.00 - 3.00 hour
Back Pressure 0.490 - 0.979 MPa71.1 - 142 psi
Screw Speed 80 - 120 rpm80 - 120 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PDENJ805 / 250149

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.