MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Teknor Apex Chemlon® 66CF4 Nylon 66, Conditioned, 20% Carbon Reinforced
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 20% Carbon Fiber Filled

Material Notes: Notes: 66CF is s 20% carbon fiber filled grade of nylon 66. It offers outstanding strength and stiffness – coupled with low density and improved electrical conductivity of molded parts. It is suitable for applications such as bearings and mechanical parts.

Availability: Europe

Fillers/Reinforcement: Carbon Fiber, 20% Filler by Weight

Features: High Stiffness; High Strength; Low Density

Uses: Bearings; Machine/Mechanical Parts

Processing Method: Injection Molding

Information provided by Teknor Apex

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.22 g/cc0.0441 lb/in³ISO 1183
Moisture Absorption at Equilibrium 2.2 %2.2 %50% RH; ISO 62
Linear Mold Shrinkage 0.0020 - 0.010 cm/cm0.0020 - 0.010 in/inISO 294-4
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 150 MPa21800 psiISO 527-2
Elongation at Break 4.1 %4.1 %ISO 527-2
Tensile Modulus 8.41 GPa1220 ksiISO 527-2
Flexural Strength 259 MPa37600 psiISO 178
Flexural Modulus 7.52 GPa1090 ksiISO 178
Izod Impact, Notched (ISO) 7.56 kJ/m²3.60 ft-lb/in²ISO 180/A
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 280 - 295 °C536 - 563 °F
Middle Barrel Temperature 280 - 295 °C536 - 563 °F
Front Barrel Temperature 280 - 295 °C536 - 563 °F
Melt Temperature 285 - 300 °C545 - 572 °F
Mold Temperature 90.0 - 100 °C194 - 212 °F
Drying Temperature 80.0 °C176 °F
Dry Time 2.00 hour2.00 hour

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PTEKNQ0671 / 237162

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.