MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

TIMET 6-6-2 Titanium Alloy (Ti-6Al-6V-2Sn), Annealed
Categories: Metal; Nonferrous Metal; Titanium Alloy; Alpha/Beta Titanium Alloy

Material Notes: TIMETAL 6-6-2 offers improved strength properties and greater depth hardenability compared with TIMETAL 6-4.

Data provided by TIMET.

Key Words: UNS R56620
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 4.53 g/cc0.164 lb/in³Typical
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 1090 MPa158000 psiTypical
Tensile Strength, Yield 1005 MPa
@Strain 0.2 %
145800 psi
@Strain 0.2 %
Typical
Elongation at Break 10 %10 %Typical
Modulus of Elasticity 115 GPa16700 ksiTypical
Fatigue Strength 490 MPa71100 psiLimit; test specifics not reported
 
Thermal PropertiesMetricEnglishComments
Beta Transus 1050 °C1920 °F
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 6.0 %6.0 %
Copper, Cu 0.50 %0.50 %
Iron, Fe 0.50 %0.50 %
Tin, Sn 2.0 %2.0 %
Titanium, Ti 85 %85 %Calculated as remainder
Vanadium, V 6.0 %6.0 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
TIMET 6-6-2 Titanium Alloy (Ti-6Al-6V-2Sn), Solution Treated and Aged
Titanium Ti-6Al-6V-2Sn (Ti-6-6-2) Annealed
TIMET TIMETAL® 6-2-4-6 Titanium Alloy (Ti-6Al-2Sn-4Zr-6Mo), Typical
Haynes 556® alloy, cold rolled, solution annealed sheet, 0.8-2.8 mm thick
Magnesium Elektron Elektron® W7 Magnesium Alloy Welding Rod Composition

NTIME662 / 19334

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.