MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Nouryon Ethylan TD1085
Categories: Other Engineering Material

Material Notes: Ethoxylated alcohol mainly used as wetting and dispersing agent in several applications

Information provided by Nouryon

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.03 g/cc0.0372 lb/in³
pH 5.0 - 7.05.0 - 7.01% in water
Viscosity 210 cP210 cP
Surface Tension 27 dynes/cm27 dynes/cmaccording to Du Noüy, 25°C, 0.1%; DIN 53914
 
Thermal PropertiesMetricEnglishComments
Pour Point 1.00 °C33.8 °F
Flash Point >= 100 °C>= 212 °F
 
Component Elements PropertiesMetricEnglishComments
H2O, Water 14 - 16 %14 - 16 %
 
Descriptive Properties
AppearanceClear/slight opalescent liquid
Clear point4 °C
Cloud point77°C1% in water
Color= 50 Hazen
Content (%)85Active content
Foam Height according to Ross-Miles115 mmimmediately, 50°C, 0.05%
 35 mmafter 5 min, 50°C, 0.05%
HLB13.7Griffin
Wetting power11 secaccording to Draves, 25°C, 0.1%

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PNOURY577 / 286100

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.