MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Phillips 66 Koolkut® ACM ISO Grade 10
Categories: Fluid; Lubricant

Material Notes: Koolkut ACM is a low-viscosity, chlorine-free, inactive cutting oil developed for light-duty machining of aluminum, copper, magnesium and other soft, non-ferrous metals. It is specially formulated with high-quality base oils to provide good cooling and wetting of the cutting tool and workpiece, while penetrating and protecting them against corrosion and the formation of oxides. Koolkut ACM is clear, allowing good observation of the machining operation. It is noncorrosive to copper and copper alloys and nonstaining to aluminum, magnesium and other soft metals.

Applications:

  • Grinding
  • Milling
  • Rolling
  • Turning

    Features/Benefit:

    • Excellent performance in machining soft metals
    • Noncorrosive and nonstaining
    • Helps extend cutting tool life
    • Good surface finish
    • Chlorine-free for reduced environmental impact
    • Clear for good visibility of the machining operation

    Information provided by Phillips 66 Lubricants.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.901 g/cc0.901 g/cc
Density 0.899 g/cc0.0325 lb/in³
Kinematic Viscosity at 40°C (104°F) 10.3 cSt10.3 cSt
Kinematic Viscosity at 100°C (212°F) 63 cSt63 cSt
ASTM Color 1.51.5ASTM D1500
 
Thermal PropertiesMetricEnglishComments
Pour Point -57.0 °C-70.6 °F
Flash Point 154 °C309 °FCOC
 
Component Elements PropertiesMetricEnglishComments
Sulfur, S 0.020 %0.020 %Total
 
Descriptive Properties
Copper Corrosion1aASTM D130

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
AISI 440 Stainless Steel
Shandong Rike Chemical ACM-1 PVC Impact Modifier ACM Resin
Lanxess Rhenogran® KST-50/ACM (GE 1857) Rubber Processing Aid
Lanxess Rhenogran® Diuron-80/ACM Rubber Processing Aid
ExxonMobil Bicor® 170 ASB-X OPP Film

WCON5262 / 198515

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.