MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Domo TechnylStar™ A205 F Natural S PA66, Eh 50
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, Unreinforced

Material Notes: TECHNYLSTAR A205 F NATURAL S is a polyamide 6.6 with low viscosity for fast cycle molding.

Colors: it is supplied in natural color.

Available in: Latin America and North America

Main Properties: High Fluidity, V2 UL 94 Classification and Glow wire Resistance

Applications: This product is indicated for various applications at automotive and electric & electronic industries.

DOMO Chemicals has acquired Solvay’s Performance Polyamides Business in Europe.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.15 g/ccISO 1183/A
Water Absorption 1.5 %
@Temperature 23.0 °C,
Time 86400 sec
ISO 62
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 79.0 MPaISO 527
Tensile Modulus 2270 MPaISO 527
Charpy Impact, Notched 6.60 kJ/m²ISO 179
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+13 ohm-cmCEI 93
Dielectric Constant 3.2CEI 250
Dielectric Strength 26.0 kV/mmCEI 93
Dissipation Factor 0.080CEI 250
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 153 °CISO 75

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Domo TechnylStar™ A205 F Natural S PA6, Eh 0
Domo TECHNYL® A 205F PA66, DRY
Domo Technyl® A 205F Nylon 66, EH0

PRHOD818 / 138049

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.