Clyrell RC649U is a clarified development polypropylene resin with antistatic additivation used in injection molding. It features an excellent combination of high stiffness and high transparency that enables customers to achieve excellent performances and aesthetic appearance which appeals to end users. Status: Developmental Availability: Africa-Middle East; Europe Application: Clear Containers; Housewares; Sports, Leisure & Toys Market: Consumer Products; Rigid Packaging Processing Method: Injection Molding Attribute: Contains Antistat; High Stiffness; High Transparency Information provided by LyondellBasell. |