MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Chemours Viton® RC Process Aid  (discontinued **)
Categories: Other Engineering Material; Additive/Filler for Polymer; Polymer

Material Notes: Description: Viton® FreeFlow™ RC is a new processing additive for narrow molecular weight LLDPE. This material will eliminate melt fracture, lower extrusion pressure, reduce extrusion torque, and reduce die buildup. Viton® FreeFlow™ RC combines a lubricant to accelerate die conditioning with the die cleaning properties of Viton® FreeFlow™ SC. This combination provides a highly efficient processing additive when rapid die conditioning is required. Viton® FreeFlow™ RC also incorporates improved chemistry to reduce interactions with other formulation ingredients. It is a superior choice for making combined masterbatches with pigments or antiblock. Due to the low lubricant level, no effects on surface properties of the finished products are expected.

Advantages:

  • Improved rates of conditioning when starting up new formulations on clean dies or purged systems
  • Improved additive efficiency particularly on lines where frequent formula changes are made or in formulas containing multiple additives
  • Extended running time between die cleanings
  • Improved performance in combined masterbatches with pigments
  • Improved economics
  • Approved for food contact and potable water applications
  • Simplified analytical procedures for quality control

Information provided by manufacturer.

Chemours was formed from former DuPont performance chemicals businesses, including the Viton product line, in 2015. This specific grade had been discontinued prior to the spinoff.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.06 - 1.12 g/cc
 
Descriptive Properties
AppearanceWhite, free-flowing powder
Package Stability4 yr
Packaging25 kg carton

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PDVDA68 / 34037

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.