MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Trinseo MAGNUM™ 3404 Smooth ABS
Categories: Polymer; Thermoplastic; ABS Polymer; Acrylonitrile Butadiene Styrene (ABS), Extruded

Material Notes: Product Description: MAGNUM™ 3404 Smooth is an excellent general purpose extrusion/thermoforming resin with outstanding processability. The mass (continuous process) ABS technology ensures an ABS resin that combines excellent processability with a stable light base color that is ideal for self-coloring. The new MAGNUM ‘Smooth Series’ resins have an ultra low particulate content, which results in a superb surface finish that will enable our customers to produce parts with excellent aesthetics at a lower total cost.
Applications: Transportation; Sanitary ware; Signage; Furnishings; Protective covers; Marine; Recreational vehicles

Availability: Europe; Latin America; North America

Features: Good Processability; Good Surface Finish; Medium Heat Resistance; Medium Impact Resistance

Uses: Furniture; General Purpose; Marine Applications; Protective Coverings

Form: Pellets

Processing Method: Blow Molding; Injection Molding; Profile Extrusion; Sheet Extrusion; Thermoforming

Information provided by Trinseo

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.05 g/cc0.0379 lb/in³ISO 1183
Linear Mold Shrinkage 0.0040 - 0.0070 cm/cm0.0040 - 0.0070 in/inISO 294-4
Melt Flow 6.6 g/10 min
@Load 10.0 kg,
Temperature 220 °C
6.6 g/10 min
@Load 22.0 lb,
Temperature 428 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 43.0 MPa6240 psiISO 527-2/50
Elongation at Yield 2.7 %2.7 %ISO 527-2/50
Tensile Modulus 2.15 GPa312 ksiIOS 527-1/1
Flexural Strength 70.3 MPa10200 psiISO 178
Flexural Modulus 2.10 GPa305 ksiISO 178
Charpy Impact, Notched 1.81 J/cm²8.60 ft-lb/in²Injection Molded; ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 101 °C214 °FUnannealed; ISO 75-2/A
Vicat Softening Point 102 °C216 °FISO 306/B50
Flammability, UL94  HB
@Thickness 1.52 mm
HB
@Thickness 0.0600 in
 HB
@Thickness 3.05 mm
HB
@Thickness 0.120 in
 
Processing PropertiesMetricEnglishComments
Drying Temperature 80.0 - 90.0 °C176 - 194 °F
Dry Time 2.00 - 4.00 hour2.00 - 4.00 hour

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PTRINSE1536 / 312229

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.