MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Syensqo (Solvay Specialty Polymers) Ryton® XE3500BL PPS Alloy
Categories: Polymer; Thermoplastic; Polyphenylene Sulfide (PPS)

Material Notes: Ryton® XE3500BL unfilled polyphenylene sulfide alloy compound for extrusion and blow molding provides excellent mechanical strength, ductility, toughness and chemical resistance.

Features: Chemical Resistant; Ductile; Good Toughness; High Strength

Extrusion notes: Storage:
Bags should be preferably stored in a dry room at a maximum temperature of 60°C (140°F) and should be protected from possible damage.

Pre-Drying:
This resin should be dried prior to extrusion following the recommendations found in the processing guide.

Information provided by Solvay Specialty Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.20 g/cc0.0434 lb/in³ISO 1183
Water Absorption 0.10 %
@Time 86400 sec
0.10 %
@Time 24.0 hour
ASTM D570
Melt Flow 1.0 g/10 min1.0 g/10 minProcedure B; ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 40.0 MPa5800 psiASTM D638
Elongation at Break 80 %80 %ASTM D638
Tensile Modulus 1.50 GPa218 ksiISO 527-2
Flexural Strength 60.0 MPa8700 psiASTM D790
Flexural Modulus 1.50 GPa218 ksiISO 178
Izod Impact, Notched (ISO) 50.0 kJ/m²23.8 ft-lb/in²Notch A; ISO 180
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant  3.1
@Frequency 1000 Hz
3.1
@Frequency 1000 Hz
ASTM D150
 3.1
@Frequency 1e+6 Hz
3.1
@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength 24.0 kV/mm610 kV/inASTM D149
Dissipation Factor  0.0020
@Frequency 1000 Hz
0.0020
@Frequency 1000 Hz
ASTM D150
 0.0050
@Frequency 1e+6 Hz
0.0050
@Frequency 1e+6 Hz
ASTM D150
Arc Resistance 120 sec120 secASTM D495
 
Thermal PropertiesMetricEnglishComments
CTE, linear  80.0 µm/m-°C
@Temperature -50.0 - 50.0 °C
44.4 µin/in-°F
@Temperature -58.0 - 122 °F
ISO 11359-2
 150 µm/m-°C
@Temperature 100 - 200 °C
83.3 µin/in-°F
@Temperature 212 - 392 °F
ISO 11359-2
Thermal Conductivity 0.200 W/m-K1.39 BTU-in/hr-ft²-°FISO 8302
Flammability, UL94 V-0
@Thickness 1.60 mm
V-0
@Thickness 0.0630 in
 
Descriptive Properties
AvailabilityAsia Pacific
 Europe
 Latin America
 North America
ColorBlack
FormsPellets
RoHS ComplianceYes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSOL8Y4454 / 280254

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.