MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Cadmium Germanium Phosphide, CdGeP2
Categories: Ceramic; Phosphide/Pnictide; Other Engineering Material; Semiconductor

Key Words: Pnictide; Semiconductor
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 4.48 g/cc
a Lattice Constant 5.741 Å
c Lattice Constant 10.755 Å
 
Mechanical PropertiesOriginal ValueComments
Knoop Microhardness 5650N/mm²
 
Electrical PropertiesOriginal ValueComments
Band Gap 1.8 eV
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 11.0 W/m-K
Melting Point 776 °C
Heat of Formation 289 kJ/mol
 
Descriptive Properties
Crystal StructureTetragonalChalcopyrite Structure - Space Group I(-4)2d

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Cadmium Germanium Arsenide, CdGeAs2
Cadmium Oxide, CdO
Cadmium Selenide, CdSe, Cubic
Bismuth Telluride, Bi2Te3 (Tellurobismuthite)
Cadmium Sulfide, CdS, Cubic (Hawleyite)

DSEM28 / 2943

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.